It provides outstandingt performance in mirror bonding and glass installation. Has excellent adhesion to plastic, wooden, and metal profiles in PVC joinery applications, as well as to tile, glass, and ceramic surfaces.
- Surface to be applied must be dry and clean, free of dust, dirt, and grease.
- Tape both sides of the application area.
- Cut the cartridge tip and place it in the gun.
- Cut the tip of the nozzle, attach it to the cartridge, and apply the silicone.
- Clean uncured silicone residue around with soapy water.
- Protect from water for 3 hours after application.
| Chemical Basis |
Neutral |
| Skin Forming Time |
5-20 min |
| Curing Rate |
4-5 mm/day |
| Density |
1,01 g/cm3 ±0,01 |
| Elongation at Break |
% 200 ± 30 |
| Tensile Strength |
0,6 ±0,1 N/mm2 |
| Hardness Shore A |
24 |
| Thermal Resistance |
-40ºC to +180ºC |
| Application Temperature |
+5ºC / +40ºC |
| Storage Temperature |
0ºC / +35ºC |
| Shelf life |
18 months |